Polymer Property : Glass Transition Temp, Tg = 82.4 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 28.0 °C
82.4 °F
ASTM E1545-00
DSM Somos® WaterClear® 10120 Epoxy Resin for Stereolithography  (discontinued **)
DescriptionDSM Somos® 10120 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us..
Glass Transition Temp, Tg 28.0 °C
82.4 °F
TM R050-25
Resinlab® EP1200 Black Casting Resin
Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re..