Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 9.00 °C | 48.2 °F | |
Styron DL 475NA Functionalized SB Performance Features: Excellent alkaline stability, excellent adhesion and strengthApplications: MasticsNorth AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | 9.00 °C | 48.2 °F | |
Styron XQ 97901.00 Modified SB Performance Features: General purpose heat sealable, low odor, high water resistance, casein compatibility, good adhesion to cellulosic materialsApplications: Foil Laminated (FSK), Heat Sealable, La.. |
|||
Glass Transition Temp, Tg | 9.00 °C | 48.2 °F | |
Styron DL 233NA Functionalized SB Performance Features: Isocyanate adhesive modifier, good bonding to paperApplications: General Purpose Adhesive, Lamination (Metalized Paper) and Wood Adhesive (EPI)North AmericaInformation provided.. |
|||
Glass Transition Temp, Tg | 9.00 °C | 48.2 °F | |
Styron DL 233NA Functionalized SB Performance Features: Excellent binding strength and durability, excellent acoustic propertiesApplications: Dust Control, Soil Stabilization and Sound DampeningNorth AmericaInformation provided by S.. |