Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 102 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C

@Thickness 6.40 mm
216 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
Deflection Temperature at 0.46 MPa (66 psi) 102 °C

@Thickness 6.40 mm
216 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific)
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
Deflection Temperature at 0.46 MPa (66 psi) 102 °C

@Thickness 6.40 mm
216 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
Deflection Temperature at 0.46 MPa (66 psi) 102 °C

@Thickness 12.7 mm
216 °F

@Thickness 0.500 in
Annealed; ASTM-D648
Ineos ABS Lustran® 308 ABS, Medical Grade
Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi..
Deflection Temperature at 0.46 MPa (66 psi) 102 °C

@Thickness 12.7 mm
216 °F

@Thickness 0.500 in
Annealed; ASTM-D648
Ineos ABS Lustran® 633 ABS, Injection Molding Grade
Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical ..
Deflection Temperature at 0.46 MPa (66 psi) 102 °C

@Thickness 3.20 mm
216 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+HIPS (Europe-Africa-Middle East)
LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi.
Deflection Temperature at 0.46 MPa (66 psi) 102 °C

@Thickness 3.20 mm
216 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+PS
LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi.