Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 120 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C

@Thickness 6.40 mm
248 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL PVX516 PPE
PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT
Deflection Temperature at 0.46 MPa (66 psi) 120 °C

@Thickness 6.40 mm
248 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific)
Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized