Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 134 °C

@Thickness 6.40 mm
273 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL LTA1350 PPE+PS
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Deflection Temperature at 0.46 MPa (66 psi) 134 °C

@Thickness 6.40 mm
273 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Deflection Temperature at 0.46 MPa (66 psi) 134 °C

@Thickness 6.40 mm
273 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL LTA5020 PPE+PS
Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Deflection Temperature at 0.46 MPa (66 psi) 134 °C

@Thickness 6.40 mm
273 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Noryl N1251 PPE+PS
ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 0.46 MPa (66 psi) 134 °C

@Thickness 6.40 mm
273 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL NH5120 PPE+PS
Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re..
Deflection Temperature at 0.46 MPa (66 psi) 134 °C

@Thickness 6.40 mm
273 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..