Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 138 °C @Thickness 6.40 mm |
280 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Valox® 357 PBT PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 138 °C @Thickness 6.40 mm |
280 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 357 PBT+PC PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |