Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C

@Thickness 6.35 mm
163 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M3500 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C

@Thickness 6.35 mm
163 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M4805 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C

@Thickness 6.35 mm
163 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C

@Thickness 6.35 mm
163 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C

@Thickness 6.35 mm
163 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C

@Thickness 6.35 mm
163 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding MR900 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C

@Thickness 6.35 mm
163 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M4820 Polyvinyl Chloride, Rigid (PVC, Rigid)