Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 83.9 °C @Treatment Temp. 60.0 °C, Thickness 3.18 mm |
183 °F @Treatment Temp. 140 °F, Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy) Physical properties based on Geon HTX L1502 white 1000.Information provided by PolyOne |