Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C

@Treatment Temp. 50.0 °C,
Thickness 3.18 mm
192 °F

@Treatment Temp. 122 °F,
Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ HTX E1502 Polyvinyl Chloride Alloy (PVC Alloy)
VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C

@Thickness 3.18 mm
192 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ HTX Ultra LA426G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Higher gloss version of Geon HTX Ultra LA426Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426G Black 2880.Information provided by Pol..