Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 133 °C

@Thickness 6.40 mm
271 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL NH5020 PPE+PS
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
Deflection Temperature at 0.46 MPa (66 psi) 133 °C

@Thickness 6.40 mm
271 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
Deflection Temperature at 0.46 MPa (66 psi) 133 °C

@Thickness 6.40 mm
271 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..