Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C

@Thickness 3.20 mm
187 °F

@Thickness 0.126 in
ASTM D648
LG Chemical XG568 MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C

@Thickness 3.20 mm
187 °F

@Thickness 0.126 in
ASTM D648
LG Chemical XG569C MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C

@Thickness 6.40 mm
187 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL N750 PPE+PS
ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications.