Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 110 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C

@Thickness 6.40 mm
230 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS
PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications.
Deflection Temperature at 1.8 MPa (264 psi) 110 °C

@Thickness 6.40 mm
230 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Asia Pacific)
PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications.
Deflection Temperature at 1.8 MPa (264 psi) 110 °C

@Thickness 6.40 mm
230 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® MC8002 PC+ABS
AUTOMOTIVE. Low viscosity, high impact and ductility.
Deflection Temperature at 1.8 MPa (264 psi) 110 °C

@Thickness 6.40 mm
230 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® MC8002 PC+ABS (Asia Pacific)
AUTOMOTIVE. Low viscosity, high impact and ductility.