Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 75.6 °C

@Treatment Temp. 50.0 °C,
Thickness 3.18 mm
168 °F

@Treatment Temp. 122 °F,
Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO..