Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 173 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.3 °C

@Thickness 3.18 mm
173 °F

@Thickness 0.125 in
Compression Molded, Annealed at 60 deg.C; ASTM D648
PolyOne Geon™ Vinyl Dry Blend E7009 Polyvinyl Chloride, Rigid (PVC, Rigid)
Recommended for whites and light pastel colors only. Not to be used for darker colors.Physical properties based on Geon E7009 white 1024 lot# UTCX 57572Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 78.3 °C

@Thickness 3.18 mm
173 °F

@Thickness 0.125 in
Compression Molded, Annealed at 60 deg.C; ASTM D648
PolyOne Geon™ Vinyl Dry Blend E7506 Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon E7506 is recommended for whites and light pastel colors only. Performs well in extrusion blow molding and high rate fencing capstock applications.Physical properties based on Geon E7506 white 1..
Copyright © lookpolymers.com All Rights Reserved