Deflection Temperature at 1.8 MPa (264 psi) 80.6 °C

@Thickness 12.7 mm
177 °F

@Thickness 0.500 in
Unannealed; ASTM-D648
Ineos ABS Lustran® 451 ABS, Injection Molding Grade
Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss.