Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C @Thickness 12.7 mm |
215 °F @Thickness 0.500 in |
Annealed (24h @ 185°F); ASTM-D648 |
Ineos ABS Lustran® 451 ABS, Injection Molding Grade Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss. |