Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 221 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C

@Thickness 6.40 mm
221 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East)
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.
Deflection Temperature at 1.8 MPa (264 psi) 105 °C

@Thickness 6.40 mm
221 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.
Deflection Temperature at 1.8 MPa (264 psi) 105 °C

@Thickness 3.20 mm
221 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics Noryl EN110 PPE+PS (Asia Pacific)
Medium heat, extrusion grade PPO/HIPS alloy.This data was supplied by SABIC-IP for the Asia Pacific region.