Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 262 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 6.40 mm
262 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS
PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance.
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1200-08 Polycarbonate Resin
Description: LUPOY PC 1200-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1200-10 Polycarbonate Resin
Description: LUPOY PC 1200-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1201-08 Polycarbonate Resin
Description: LUPOY PC 1201-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1201-10 Polycarbonate Resin
Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1301-10 Polycarbonate Resin
Description: LUPOY PC 1301-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1301V-10 Polycarbonate Resin
Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength..
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1621-02 Polycarbonate Resin
Description: LUPOY PC 1621-02 resin is designed for large injection stretch blow molding and extrusion blow molding parts. It exhibits an excellent physical property balance of heat resistance, tran..
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 3010-10 Polycarbonate Resin
Description: LUPOY PC 3010-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 3030-10 Polycarbonate Resin
Description: LUPOY PC 3030-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1201HP-08 Polycarbonate Resin
Description: LUPOY PC 1201HP-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1300-10 Polycarbonate Resin
Description: LUPOY PC 1300-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1302-10 Polycarbonate Resin
Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin
Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1302UV-08 Polycarbonate Resin
Description: LUPOY PC 1302UV-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1303-10 Polycarbonate Resin
Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 4.00 mm
262 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1303AH-10 Polycarbonate Resin
Description: LUPOY PC 1303AH-10 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
Copyright © lookpolymers.com All Rights Reserved