Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 277 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 4.00 mm
277 °F

@Thickness 0.157 in
Annealed; ASTM D648
LG Chemical Lupoy 1301EP30 Polycarbonate Resin
Description: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 4.00 mm
277 °F

@Thickness 0.157 in
Annealed; ASTM D648
LG Chemical Lupoy 1302EP-30 Polycarbonate Resin
Description: LUPOY PC 1302EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 4.00 mm
277 °F

@Thickness 0.157 in
Annealed; ASTM D648
LG Chemical Lupoy 1303EP-30 Polycarbonate Resin
Description: LUPOY PC 1303EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 4.00 mm
277 °F

@Thickness 0.157 in
Annealed; ASTM D648
LG Chemical Lupoy 3010-30 Polycarbonate Resin
Description: LUPOY PC 3010-30 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..