Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C @Thickness 6.35 mm |
158 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C @Thickness 6.35 mm |
158 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C @Thickness 6.35 mm |
158 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding MR900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C @Thickness 3.18 mm |
158 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ SF M7000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C @Thickness 3.18 mm |
158 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C @Thickness 3.18 mm |
158 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ SF M7020 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |