Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 3.20 mm |
172 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl ENV85 PPE+PS (Asia Pacific) Low heat, flame retardant, extrusion grade PPO/HIPS alloy.Internal flammability results only.Not a UL recognised material.This data was supplied by SABIC-IP for the Asia Pacific region. |