Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 36.1 °C

@Thickness 3.18 mm
97.0 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ L4605 Green 5765 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 36.1 °C

@Thickness 3.18 mm
97.0 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ L4605 Red 7640 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 36.1 °C

@Thickness 3.18 mm
97.0 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ L4605 Red 7640 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid)
Information provided by PolyOne