Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 38.0 °C @Pressure 1.80 MPa |
100 °F @Pressure 261 psi |
ISO 57B-1 |
Iran Petrochemical (PCC) MF3820 High Density Polyethylene MF-3820 is a high molecular weight high density polyethylene. Application: bottle extrusion.Information provided by Iran Petrochemical Commercial Co. |