Thermal Properties Metric English Comments
Heat Distortion Temperature 43.0 °C

@Pressure 1.80 MPa
109 °F

@Pressure 261 psi
ISO 57B-1
Iran Petrochemical (PCC) HB5020 High Density Polyethylene
HB-5020 is a high molecular weight high density polyethylene.Applications: extrusion blow moldingInformation provided by Iran Petrochemical Commercial Co.