Polymer Property : CTE, linear, Transverse to Flow = 109 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 80.0 - 196 µm/m-°C
44.4 - 109 µin/in-°F
Average value: 107 µm/m-°C Grade Count:8
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..