Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 11.9 µm/m-°C

@Temperature 20.0 °C
6.61 µin/in-°F

@Temperature 68.0 °F
Crosswise; ASTM D696
G-10 Fiberglass Epoxy Laminate Sheet
This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e..