Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 114 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -40.0 - 40.0 °C
63.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal
LNP LUBRICOMP* KP004 is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -30.0 - 30.0 °C
63.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66
LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -30.0 - 30.0 °C
63.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66
LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI..
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature 23.0 - 60.0 °C
63.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp HF00ASU PA11 (Europe-Africa-Middle East)
LNP* THERMOCOMP* HF00ASU is a compound based on PA11 resin containing Glass Fiber. Added features include; Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid..
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature 23.0 - 60.0 °C
63.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp MB006SU PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MB006SU is a compound based on Polypropylene resin containing Glass Bead. Added features include: Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Af..
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -30.0 - 30.0 °C
63.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10
LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber.
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature 23.0 - 60.0 °C
63.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starpylen MB006SU PP, Glass Bead Filled, Injection Molding Resin
Starpylen MB006SU is a Glass Bead Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature -30.0 - 30.0 °C
63.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP VERTON PX06418 PA 6
LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural.
Copyright © lookpolymers.com All Rights Reserved