Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66
(Unverified Data**) Zytel® ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance, high productivity and laser markability.Information provided by DuPont |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 20.0 °C |
66.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K230-HPV8 Impact Modified Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced PA 6-Copolymer, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 4235 Z 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, impact modified |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® S 7926 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 1505 000000 PBT PBT, non-reinforced, injection molding, extrusion |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 60.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MB006SXP PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006SXP is a compound based on Polypropylene resin containing Glass Bead. Added featurs include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 80.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East) VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 20.0 °C |
66.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359-2 |
Polyplastics Tepcon M90 Acetal-copolymer (POM), General Information provided by PolyPlastics. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 3105A Polybutylene Terephthalate (PBT), Epoxy adhesion improved, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-15 PA6-GF15 Product description: Grilon BG-15 is a heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon BG-15 has the following important properties: Good surface finishGood b.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100TE NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100TE NC010 (formerly DE20580) is a high viscosity toughened acetal homopolymer with very low VOC emissions. Processing met.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66 + Nylon 6
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 + Polyamide 6 Zytel 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was develop.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66
(Unverified Data**) Super Toughened Heat Stabilized Polyamide 66 Zytel ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance high productivity and laser marka.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 60.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TR 90 NZZ nat PAMACM12-I Product description: Grilamid TR 90 NZZ natural is an amorphousthermoplastic polyamide, based on aliphatic and cycloaliphatic units. Grilamid TR 90 NZZ natural offers a variety of interesting proper.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBAFORM C 520.0 POM Copolymer unreinforced POMInformation provided by BARLOG plastics GmbH. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® HP90X Acetal Co-polymer (POM), High stiffness, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |