Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 137 - 168 µm/m-°C
76.1 - 93.3 µin/in-°F
Average value: 148 µm/m-°C Grade Count:3
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..