Polymer Property : CTE, linear, Transverse to Flow = 185 µm/m-°C
Polymer Property :
CTE, linear, Transverse to Flow =
185 µm/m-°C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
CTE, linear, Transverse to Flow
185
µm/m-°C
103
µin/in-°F
ISO 11359-1/-2
DSM Arnitel® EM631 TPC-ET
Extrusion Grade