Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 203 µm/m-°C
113 µin/in-°F
z direction
Arlon IsoClad 933 Non-Woven Fiberglass Reinforced PTFE
Traditional - Highest Performance, PTFE Coated Light Woven Glass Styles, Interdispersed PTFE FilmInformation provided by Arlon Materials for Electronics (MED).