Polymer Property : CTE, linear, Transverse to Flow = 22.6 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 22.6 µm/m-°C

@Temperature -30.0 - 30.0 °C
12.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp OC008A PPS - Branched
LNP* Thermocomp* OC008A is a compound based on Branched Polyphenylene Sulfide containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region.