Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 7.24 µm/m-°C

@Temperature -30.0 - 30.0 °C
4.02 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RC008H PA 66
LNP THERMOCOMP* RC008H is a compound based on Nylon 66 resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.