Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 4.44 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
4.44 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp DEL34 PC (Europe-Africa-Middle East)
LNP* Lubricomp* DEL34 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP f..
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
4.44 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP545 Carbon Fiber  (discontinued **)
Description: NP545 is composed of carbon fiber fabric and an epoxy resin system. It has excellent moisture resistance and physical properties. Potential uses include fixtures and gage systems, high ..
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
4.44 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66
LNP* STAT-KON* RFD03 is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material is: Electrically Conductive.
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature -40.0 - 150 °C
4.44 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI
LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding.
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
4.44 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66
LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
4.44 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66
LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized.
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
4.44 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP DC0049XF PC
LNP* THERMOCOMP* DC0049XF is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature 23.0 °C
4.44 µin/in-°F

@Temperature 73.4 °F
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature 23.0 °C
4.44 µin/in-°F

@Temperature 73.4 °F
Alliance C-7 Strontium Ferrite Ceramic Magnetic Material
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature 23.0 °C
4.44 µin/in-°F

@Temperature 73.4 °F
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature 23.0 °C
4.44 µin/in-°F

@Temperature 73.4 °F
Alliance C-8 Strontium Ferrite Ceramic Magnetic Material
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature 23.0 °C
4.44 µin/in-°F

@Temperature 73.4 °F
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature 23.0 °C
4.44 µin/in-°F

@Temperature 73.4 °F
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature 23.0 °C
4.44 µin/in-°F

@Temperature 73.4 °F
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material
CTE, linear, Transverse to Flow 8.00 µm/m-°C

@Temperature 23.0 °C
4.44 µin/in-°F

@Temperature 73.4 °F
Alliance C-8B Strontium Ferrite Ceramic Magnetic Material