Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 42.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 34.0 - 42.0 µm/m-°C
18.9 - 23.3 µin/in-°F
Average value: 38.7 µm/m-°C Grade Count:3
Overview of materials for Thermoset Polyurethane, Liquid, Quartz Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid, Quartz Filled". Each property range of values reported is minimum and ma..