Polymer Property : CTE, linear, Transverse to Flow = 47.8 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 30.0 - 86.0 µm/m-°C
16.7 - 47.8 µin/in-°F
Average value: 54.6 µm/m-°C Grade Count:8
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..