Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 91.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® FR15U ABS
Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60).
CTE, linear, Transverse to Flow 91.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific)
Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing.
CTE, linear, Transverse to Flow 91.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics GELOY CR7020 ASA
ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact.
CTE, linear, Transverse to Flow 91.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific)
ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact.
CTE, linear, Transverse to Flow 91.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics GELOY CR7520 ASA
General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL.
CTE, linear, Transverse to Flow 91.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
51.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Noryl N190HX PPE+PS
High gloss. 182F (83C) HDT. UL94 V-0/5VA rated.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 91.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific)
ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL.