Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 57.5 - 59.5 µm/m-°C

@Temperature -30.0 - 30.0 °C
31.9 - 33.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP WH0270F PBT
LNP* Thermocomp* WH0270F is a dense compound based on PBT.
CTE, linear, Transverse to Flow 57.5 - 59.5 µm/m-°C

@Temperature -30.0 - 30.0 °C
31.9 - 33.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp WH0270FX_WH5A289 PBT
2.7 specific gravity PBTThis data was supplied by SABIC-IP for the Americas region.