Polymer Property : CTE, linear, Transverse to Flow = 58.3 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 105 - 190 µm/m-°C
58.3 - 106 µin/in-°F
Average value: 139 µm/m-°C Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature 20.0 °C
58.3 µin/in-°F

@Temperature 68.0 °F
Covestro Bayblend® KU 2-1446 Polycarbonate + ABS Blend  (discontinued **)
Key Features:UnfilledPlatableSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bay..
CTE, linear, Transverse to Flow 105 µm/m-°C
58.3 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® B 1505 Z 000000 PBT
PBT, non-reinforced, injection molding, extrusion, impact modified
CTE, linear, Transverse to Flow 105 µm/m-°C
58.3 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® B 2505 000000 PBT
PBT, non-reinforced, injection molding, flame retardant
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature 23.0 - 80.0 °C
58.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® CL402U PBT+PC (Europe-Africa-Middle East)
XENOY CL402U has been specially developed for extrusion blowmoulding applications, where higher melt strength is desired. XENOY CL402U is a high impact material combined with good UV resistance perf..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature -30.0 - 30.0 °C
58.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON WS002I PBT
LNP* STAT-KON* WS002I is a compound based on PBT resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, High Impact.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature 20.0 °C
58.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Akulon® K224-G4U (Dry) 23% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding
Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East)
VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load..
CTE, linear, Transverse to Flow 105 - 125 µm/m-°C

@Temperature 55.0 - 160 °C
58.3 - 69.4 µin/in-°F

@Temperature 131 - 320 °F
Average value: 115 µm/m-°C Grade Count:2
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..