Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 36.0 - 60.0 µm/m-°C
20.0 - 33.3 µin/in-°F
Average value: 50.3 µm/m-°C Grade Count:14
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
CTE, linear, Transverse to Flow 50.0 - 60.0 µm/m-°C

@Temperature 20.0 °C
27.8 - 33.3 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 4221 XB Novolac Phenolic
Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group
CTE, linear, Transverse to Flow 50.0 - 60.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
27.8 - 33.3 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry)
Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF
CTE, linear, Transverse to Flow 50.0 - 60.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
27.8 - 33.3 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
CTE, linear, Transverse to Flow 50.0 - 60.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
27.8 - 33.3 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Dry)
Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas..
CTE, linear, Transverse to Flow 50.0 - 60.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
27.8 - 33.3 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
CTE, linear, Transverse to Flow 50.0 - 60.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
27.8 - 33.3 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry)
Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF