CTE, linear, Transverse to Flow 29.0 - 61.0 µm/m-°C
16.1 - 33.9 µin/in-°F
Average value: 47.7 µm/m-°C Grade Count:17
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..