Polymer Property : CTE, linear, Transverse to Flow = 62.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 34.0 - 62.0 µm/m-°C

@Temperature 55.0 - 260 °C
18.9 - 34.4 µin/in-°F

@Temperature 131 - 500 °F
Average value: 47.7 µm/m-°C Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
CTE, linear, Transverse to Flow 34.0 - 62.0 µm/m-°C

@Thickness 2.00 - 4.00 mm
18.9 - 34.4 µin/in-°F

@Thickness 0.0787 - 0.157 in
Average value: 47.7 µm/m-°C Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..