Polymer Property : CTE, linear, Transverse to Flow = 65.2 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 65.2 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DX11408 PC
LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility