CTE, linear, Transverse to Flow >= 66.8 µm/m-°C

@Temperature -30.0 - 30.0 °C
>= 37.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12
4.3 specific gravity nylon 12, clean compound system
CTE, linear, Transverse to Flow 66.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.