Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 135 µm/m-°C

@Temperature 23.0 - 60.0 °C
75.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP ML008 PP (Europe-Africa-Middle East)
LNP* LUBRICOMP* ML008 is a compound based on Polypropylene resin containing PTFE. Added Features include: Internally Lubricated.
CTE, linear, Transverse to Flow 135 µm/m-°C

@Temperature 23.0 - 60.0 °C
75.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp MX05038 PP (Europe-Africa-Middle East)
Polypropylene compound, containing miniral. Added features include High ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 135 µm/m-°C

@Temperature -30.0 - 30.0 °C
75.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP YF002 POLYESTER ELASTOMER
LNP* THERMOCOMP* YF002 is a compound based on Poyester Elastomer containing 10% Glass Fiber. Added feature of this grade is: High Modulus.
CTE, linear, Transverse to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
Covestro Baydur® GS PUR Polyurethane
Polyurethane casting system for the production of solid components. Pressureless casting into open or closed molds, fast demold times, good rot resistance. Combines easily with other materials.Infor..
CTE, linear, Transverse to Flow 135 µm/m-°C

@Temperature 23.0 - 60.0 °C
75.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starpylen MX05038 TPEX, Injection Molded
Starpylen MX05038 is a TPEX Injection Molding ResinInformation provided by Eurostar.