CTE, linear, Transverse to Flow 75.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications.
CTE, linear, Transverse to Flow 75.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Asia Pacific)
Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications.