Polymer Property : CTE, linear, Transverse to Flow = 79.4 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 143 µm/m-°C

@Temperature -30.0 - 30.0 °C
79.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU
LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 143 µm/m-°C

@Temperature 20.0 °C
79.4 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® RS 60E10TL Nylon 6 Alloy, Rigid Grade (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..
CTE, linear, Transverse to Flow 143 µm/m-°C

@Temperature 20.0 °C
79.4 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® RS 60E10 Nylon 6 Alloy, Rigid Grade (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties..