Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 147 µm/m-°C @Temperature 20.0 °C |
81.7 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 180A-28(HT) Cellulose Acetate
(discontinued **) 28% Plasticized.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Transverse to Flow | 147 µm/m-°C @Temperature -30.0 - 100 °C |
81.7 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 9710 PP SABIC® PPcompound 9710 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st.. |