Thermal Properties | Metric | English | Comments |
---|---|---|---|
Active Range | 96.0 - 343 °C | 205 - 649 °F | |
Indium Corp. Indalloy® 84003 Flux #3 High Viscosity Liquid Flux Indalloy Flux #3 is a high viscosity liquid flux formulated for the purpose of soldering aluminum. Indalloy Flux #3 also has proven to be an effective flux for soldering to NiTi (Nitinol) alloys. .. |