Thermal Properties Metric English Comments
CTE, linear -0.540 µm/m-°C

@Temperature 0.000 - 50.0 °C
-0.300 µin/in-°F

@Temperature 32.0 - 122 °F
Schott Nextrema® 724-3 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..